The purpose of the present in vitro study was to compare the two-body wear resistance of a type 3 gold alloy (Aurocast8), two lithium disilicate glass ceramics (IPS e.max CAD and IPS e.max Press), a heat-pressed feldspathic porcelain (Cerabien ZR Press), an yttria-stabilized tetragonal zirconia polycrystal ceramic (Katana Zirconia ML), and three heat-cured composite resins (Ceram.X Universal, Enamel Plus Function, and Enamel Plus HRi) opposing antagonistic cusps made out of the same restorative materials. Ten 6-mm-thick samples and 10 cusp-shaped abraders were manufactured with each test material (n=10) according to standard laboratory procedures. All sample/antagonist pairs made out of the same material were subjected to a two-body wear test in a dual-axis chewing simulator for up to 120,000 loading cycles. The total vertical wear (mm) and the total volumetric loss (mm3) for each sample/antagonist pair were calculated. Data were statistically analyzed using one-way analysis of variance tests. The total vertical wear for the gold alloy was not significantly different compared to Ceram.X Universal, Enamel Plus Function, IPS e.max CAD, and Cerabien ZR Press. Significantly increased wear values were observed for Enamel Plus HRi and IPS e.max Press. The lowest values for total vertical wear and volumetric loss were recorded on the monolithic zirconia.

Wear Evaluation of Prosthetic Materials Opposing Themselves

D'Arcangelo, C
;
Vadini, M;De Angelis, F
2018-01-01

Abstract

The purpose of the present in vitro study was to compare the two-body wear resistance of a type 3 gold alloy (Aurocast8), two lithium disilicate glass ceramics (IPS e.max CAD and IPS e.max Press), a heat-pressed feldspathic porcelain (Cerabien ZR Press), an yttria-stabilized tetragonal zirconia polycrystal ceramic (Katana Zirconia ML), and three heat-cured composite resins (Ceram.X Universal, Enamel Plus Function, and Enamel Plus HRi) opposing antagonistic cusps made out of the same restorative materials. Ten 6-mm-thick samples and 10 cusp-shaped abraders were manufactured with each test material (n=10) according to standard laboratory procedures. All sample/antagonist pairs made out of the same material were subjected to a two-body wear test in a dual-axis chewing simulator for up to 120,000 loading cycles. The total vertical wear (mm) and the total volumetric loss (mm3) for each sample/antagonist pair were calculated. Data were statistically analyzed using one-way analysis of variance tests. The total vertical wear for the gold alloy was not significantly different compared to Ceram.X Universal, Enamel Plus Function, IPS e.max CAD, and Cerabien ZR Press. Significantly increased wear values were observed for Enamel Plus HRi and IPS e.max Press. The lowest values for total vertical wear and volumetric loss were recorded on the monolithic zirconia.
File in questo prodotto:
File Dimensione Formato  
28 OD 2017. Wear Evaluation of Prosthetic Materials Opposing Themselves.pdf

Solo gestori archivio

Tipologia: PDF editoriale
Dimensione 729.58 kB
Formato Adobe PDF
729.58 kB Adobe PDF   Visualizza/Apri   Richiedi una copia
PRE-PRINT - 28 OD 2017. Wear Evaluation of Prosthetic Materials Opposing Themselves.pdf

accesso aperto

Tipologia: Documento in Pre-print
Dimensione 432.36 kB
Formato Adobe PDF
432.36 kB Adobe PDF Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11564/690018
Citazioni
  • ???jsp.display-item.citation.pmc??? 6
  • Scopus 32
  • ???jsp.display-item.citation.isi??? 32
social impact